High Quality Precision Machining Industrial Ceramic Part
Customize the industrial ceramic
- Rich production experience
- Strict quality inspection system
- Good price and after sale service
- Small tolerance
- Good surface roughness
Description
High Quality Precision Machining Industrial Ceramic Part
Properties of industrial ceramic part:
- Low density (3.75 to 3.95 g/cm3)
- Very high compressive strength (2,000 to 4,000 MPa)
- High hardness (15 to 19 GPa)
- Moderate thermal conductivity (20 to 30 W/mK)
- High corrosion and wear resistance

The advantages of industrial ceramic part:
1.High temperature resistance
Extreme high temperature stability under reducing, inert and high vacuum condition under high temperature up to 1800C.
2.High hardness
Rockwell hardness of high alumina ceramics is up to HRA80-90 which is second only to diamond and far exceeds wear-resistant steel and stainless steel.
3.Excellent wear resistance
The wear resistance of high alumina ceramics is 266 times that of manganese steel and 171.5 times that of high chromium cast iron.
Finishing ability: 
- The maximum height is 600mm
- The maximum length is 2500 mm
- The maximum CNC length is 1200 mm
Technical ability:
- Surface roughness:Ra0.1
- Tolerance:+-0.001mm
- Process: Sintering,Grinding, CNC Machining
- Cylindricity:0.004mm
- Parallelism:0.002mm
- Concentricity:0.003mm
Technical Data
| Properties | Unints | Alumina | Zirconia | Sic | Si3N4 | |||||
| 95%al2o3 | 97%al2o3 | 99%al2o3 | 99.5%al2o3 | 99.7%al2o3 | 99.99%al2o3 | |||||
| Density | g/cm3 | 3.6 | 3.75 | 3.8 | 3.9 | 3.94 | 3.95 | 6 | 2.7 | 2.8 |
| Color | - | White | White | Ivory | Ivory | Ivory | White | White/Black/Blue | Black | Gray |
| Hardness | Mohs Scale | 8.8 | 8.9 | 9 | 9 | 9 | 9 | 8.8 | 9.5 | 9 |
| Straightness | ‰ | 1 | 1 | 1 | 1 | 1 | 1 | 1 | 1 | 1 |
| Bending Strength(20°c) | Mpa | 304 | 320 | 340 | 370 | 375 | 375 | 1200 | 90 | 180 |
| Compressive Strength(20°c) | Mpa | 1910 | 2100 | 2210 | 2300 | 2300 | 2300 | 2500 | 600 | 650 |
| Water Absorption | % | ≤0.2 | ≤0.2 | ≤0.2 | ≤0.2 | ≤0.2 | ≤0.2 | 0 | 0 | 0 |
| Max Working Temperature | °c | 1500 | 1650 | 1700 | 1750 | 1750 | 1750 | 600 | 1600 | 1650 |
| Dielectric Constant 1MHZ(E) | 25°c@1MHz | 9.2 | 9.3 | 9.5 | 9.7 | 9.7 | 9.8 | 29 | 10 | 9.5 |
| Thermal Conductivity | W/m.k | 25 | 27.5 | 29 | 30 | 30 | 30 | 2.5 | 15 | 23 |
| Fracture Toughness | Mpa*m1/2 | 3.8 | 4 | 4.2 | 4.3 | 4.3 | 4.4 | 10 | 10 | 10 |
FAQ
1.Can i have a sample order? Or do you provide the free sample?
Yes, we welcome sample order to test and check the quality. For the free sample, if we have stock,
we can offer it with free, but the courier fee is to be collected.
2.Do you accept customized production based our specification?
Yes,we offer OEM and ODM service.
3.What’s the delivery time?
Usually 7 working days for standard products, 30 days for customized products.
4.What is the payment terms you accept?
T/T,LC,Western Union,moneygram are acceptable.
5.Why choose us?
- Rich production experience.
- Professional technical team.
- Strict quality inspection system.
- Good price and service.
- Fast delivery time.